Syasko V. A., Golubev S. S., Musikhin A. S.
THE HIGH VOLTAGE TESTING OF DIELECTRIC COATINGS THICKNESS
(pp. 12-17)

Abstract. The technology of applying many coatings (including paints and varnishes) involves the layering of visually indistinguishable layers that make up the coating system. However, in case of application technology violation, the number of coating layers (thickness) may not correspond to the declared. Thus, in a number of cases, it is necessary to control the number of layers of the final coating system. One of the most common methods for monitoring the continuity of coatings is the high voltages spark method of non-destructive testing. The method involves the application of a high voltage U between the electrode installed on the surface of the coating and the conductive substrate. The revealing of defect coating area provide by registering the coating breakdown. The analysis shows that the development of methods for detecting not only discontinuities, but also unacceptable thinning of dielectric coatings due to their spark breakdown, seems to be a promising direction in the development of high voltages spark testing. In relation to pulsed high voltages spark testing, the electrical mechanism of the breakdown of dielectrics based on quantum-mechanical concepts, the conditions of its occurrence, and the main relations obtained for calculating the electric strength Es and breakdown voltage Us for protective dielectric coatings are considered in detail. Comparative results of an experimental study of the proposed algorithms for calculating Es and Us, as well as methods for identifying (tolerance control) sections of paint coatings with an unacceptable minimum thickness and coating bubbles, are presented. The application of the proposed algorithms and methods will allow one hundred percent control of the continuity and unacceptable thinning of paint and varnish and similar dielectric protective coatings of the external and internal surfaces of pipelines, as well as various large area facilities.

Keywords: high voltage method, continuity, coating, thickness, electrical strength, breakdown voltage.

V. A. Syasko (Constanta LTD, St. Petersburg, Russia) E-mail: Данный адрес e-mail защищен от спам-ботов, Вам необходимо включить Javascript для его просмотра.
S. S. Golubev (Federal Agency on Technical Regulating and Metrology ROSSTANDART, Moscow, Russia) E-mail: Данный адрес e-mail защищен от спам-ботов, Вам необходимо включить Javascript для его просмотра.
A. S. Musikhin (Constanta LTD, St. Petersburg, Russia) E-mail: Данный адрес e-mail защищен от спам-ботов, Вам необходимо включить Javascript для его просмотра.

1. Unified system of protection against corrosion and aging. Coatings are paint and varnish. Groups, technical requirements and designations. (1989). Ru Standard No. GOST 9.032–74. Moscow: Izdatel'stvo standartov. [in Russian language]
2. Unified system of protection against corrosion and aging. Paint and varnish coatings. Appearance assessment method. (2016). Ru Standard No. GOST 9.407–2015. Moscow: Izdatel'stvo standartov. [in Russian language]
3. Paints and varnishes. Determination of coating thickness. (2016). Ru Standard No. GOST 31993–2013. Moscow: Izdatel'stvo standartov. [in Russian language]
4. Syas'ko V. A., Golubev S. S., Musihin A. S. (2019). Improvement of the electrospark method of non-destructive testing. Kontrol'. Diagnostika, (12), pp. 4 – 14. [in Russian language] DOI: 10.14489/td.2019.12.pp.004-014
5. Sazhin B. I. (1977). Electrical properties of polymers. 2nd ed. Leningrad: Himiya. [in Russian language]
6. Rayzer Yu. P. (1992). Gas discharge physics: a training manual. 2nd ed. Moscow: Nauka. [in Russian language]
7. Vorob'ev G. A., Poholkov Yu. P., Korolev Yu. D., Merkulov V. I. (2003). Physics of dielectrics (region of strong fields): a textbook. Tomsk: Izdatel'stvo TPU. [in Russian language]
8. Vershinin Yu. N. (2000). Electron-thermal and detonation processes during electrical breakdown of solid dielectrics. Ekaterinburg: Institut elektrofiziki UrO RAN. [in Russian language]

This article  is available in electronic format (PDF).

The cost of a single article is 350 rubles. (including VAT 18%). After you place an order within a few days, you will receive following documents to your specified e-mail: account on payment and receipt to pay in the bank.

After depositing your payment on our bank account we send you file of the article by e-mail.

To order articles please copy the article doi:

10.14489/td.2020.09.pp.012-017

and fill out the  form  

 

 

 
Rambler's Top100 Яндекс цитирования